Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Application: | Aviation, Electronics, Industrial, Medical, Chemical |
| Standard: | JIS, GB, DIN, BS, ASTM, AISI, ISO 9001 |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Grades | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
Main Chemical Composition (%) | Nickel (Ni) | 90 | Rest | Rest | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Chromium (Cr) | 10 | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Iron (Fe) | -- | ≤1.0 | ≤1.0 | Rest | Rest | Rest | |
Grades | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni15 | Cr20Ni30 |
Max. Service Temperature (°C) | 1300 | 1200 | 1250 | 1150 | 1100 | 1100 |
Melting Point (°C) | 1400 | 1400 | 1380 | 1390 | 1390 | 1390 |
Density (g/cm³) | 8.7 | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 |
Resistivity at 20℃ (μΩ·m) | -- | 1.09±0.05 | 1.18±0.05 | 1.12±0.05 | 1.00±0.05 | 1.00±0.05 |
Elongation at Rupture (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 |
Specific Heat (J/g.℃) | -- | 0.44 | 0.461 | 0.494 | 0.5 | 0.5 |
Thermal Conductivity (KJ/m.h.ºC) | -- | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 |
Coefficient of Lines Expansion (α×10-6/20~1000ºC) | -- | 18 | 17 | 17 | 19 | 19 |
Micrographic Structure | -- | Austenite | Austenite | Austenite | Austenite | Austenite |
Magnetic Properties | -- | Non-magnetic | Non-magnetic | Non-magnetic | Non-magnetic | Non-magnetic |